Skip to content
Hegazy Group
Resources

Technical Specifications

Detailed specifications for aluminum products, including chemical composition, mechanical properties, and tolerances.

What's included

  • Chemical composition ranges for common alloys (1xxx, 3xxx, 5xxx, 6xxx, 7xxx, 8xxx series).
  • Mechanical properties: tensile strength, yield strength, elongation, hardness by temper.
  • Dimensional tolerances for sheets, plates, coils, pipes, profiles, and bars.
  • Temper designations and heat treatment conditions.
  • Cross-reference between ASTM, EN, ISO, and AA designations.
01

Chemical Composition

Alloy SeriesCommon Alloy GradesSi (%)Fe (%)Cu (%)Mn (%)Mg (%)Zn (%)Other ElementsApplicable Standard
1xxx10500.06–0.080.25–0.27≤0.0007≤0.00270.0019–0.0044≤0.0025Ti 0.0187–0.0194; Al ≥99.58EN 485/515/573, EN 10204-3.1B*
3xxx30030.16–0.170.49–0.520.0556–0.05671.2289–1.250.0137–0.01460.0007–0.002Cr ≤0.005; Ti 0.0097–0.0098EN 485/515/573, EN 10204-3.1B*
5xxx5005A0.140.290.00320.06820.82930.0017Cr 0.0147; Ti 0.0124EN 485/515/573, EN 10204-3.1 / EN 15088:2005
5xxx5083≤0.250.15–0.4≤0.100.70–0.94.40–4.7—Cr 0.10–0.2; Ti ≤0.05; Na ≤0.0005; Other (each) ≤0.05, (total) ≤0.15Company technical specification
6xxx60820.950.250.040.540.640.04Cr 0.01; Ti 0.01EN 573-3, EN 755-2
6xxx60610.600.350.250.051.000.10Cr 0.10; Ti 0.05EN 573-3, EN 755-2
6xxx60630.20–0.600.350.050.050.45–0.460.05Cr 0.05; Ti 0.05EN 573-3, EN 755-2
6xxx60600.42–0.460.20–0.220.050.050.42–0.460.05Cr 0.05; Ti 0.05EN 573-3, EN 755-2
7xxx7075≤0.40≤0.501.20–2.00≤0.302.10–2.905.10–6.10Ti ≤0.20; Cr 0.18–0.28; Zr ≤0.05EN AW-7075, EN 573-3, EN 755-2
8xxx————————Technical values available upon request.

* Figures reflect ranges seen across multiple mill certificates for the same grade/temper; individual cast analysis will vary and is confirmed per certificate.

02

Mechanical Properties

AlloyTemperProduct FormTensile Strength (Rm)Yield Strength (Rp0.2)Elongation (A%)HardnessApplicable Standard
1050H14Sheet/Coil (0.5–3 mm)124–132 MPa121–130 MPa3–6%—EN 485, EN 10204-3.1B
3003H14Sheet/Coil (3 mm)150–155 MPa145 MPa3–6%—EN 485, EN 10204-3.1B
5005AH24Plate (3×1220×2440 mm)166 MPa162 MPa7%—EN 485/515/573, EN 10204-3.1
6082T6Bar (RB 26)≥320 MPa≥270 MPa≥10%≥95 HBEN 755-2, EN 573-3
6061T6Bar (RB 26)≥260 MPa≥240 MPa≥8%≥95 HBEN 755-2, EN 573-3
6063T66Bar (RB 26)≥245 MPa≥200 MPa≥8%≥80 HBEN 755-2, EN 573-3
6060T66Bar (RB 26)≥215 MPa≥160 MPa≥8%≥75 HBEN 755-2, EN 573-3
7075T6Extruded flat bar 80×50 mm≥560 MPa (tested: 651.49)≥500 MPa (tested: 600.89)≥7% (tested: 7.90%)174 HBW (tested)EN AW-7075, EN 755-2, EN 10204-3.1
Other grades——————Values depend on alloy, temper, product form, and applicable standard. Contact our technical team for confirmed data.
03

Dimensional Tolerances

Standard: EN 485-4:1993

Thickness tolerance by width band (mm)

Thickness (mm)≤ 1000 · Gr. I≤ 1000 · Gr. II> 1000 – 1250 · Gr. I> 1000 – 1250 · Gr. II> 1250 – 1600 · Gr. I> 1250 – 1600 · Gr. II> 1600 – 2000 · Gr. I> 1600 – 2000 · Gr. II> 2000 – 2500 · Gr. I> 2000 – 2500 · Gr. II> 2500 – 3000 · Gr. I> 2500 – 3000 · Gr. II> 3000 – 3500 · Gr. I> 3000 – 3500 · Gr. II
0.20 – 0.4±0.02±0.03±0.04±0.05±0.05±0.06————————
0.4 – 0.5±0.03±0.03±0.04±0.05±0.05±0.06±0.06±0.07±0.10±0.10————
0.5 – 0.6±0.03±0.04±0.05±0.06±0.06±0.07±0.07±0.08±0.11±0.11————
0.6 – 0.8±0.03±0.04±0.06±0.07±0.07±0.08±0.08±0.09±0.12±0.12————
0.8 – 1.0±0.04±0.05±0.06±0.08±0.08±0.09±0.09±0.10±0.13±0.13————
1.0 – 1.2±0.04±0.05±0.07±0.09±0.09±0.10±0.10±0.12±0.14±0.14————
1.2 – 1.5±0.05±0.07±0.09±0.11±0.10±0.12±0.11±0.14±0.16±0.16————
1.5 – 1.8±0.06±0.08±0.10±0.12±0.11±0.13±0.12±0.15±0.17±0.17————
1.8 – 2.0±0.06±0.09±0.11±0.13±0.12±0.14±0.14±0.16±0.19±0.19————
2.0 – 2.5±0.07±0.10±0.12±0.14±0.13±0.15±0.15±0.17±0.20±0.20————
2.5 – 3.0±0.08±0.11±0.13±0.15±0.15±0.17±0.17±0.19±0.23±0.23————
3.0 – 3.5±0.10±0.12±0.15±0.17±0.17±0.19±0.18±0.20±0.24±0.24————
3.5 – 4.0±0.15±0.15±0.20±0.20±0.22±0.22±0.23±0.23±0.25±0.25±0.34±0.34±0.38±0.38
4.0 – 5.0±0.18±0.18±0.22±0.22±0.24±0.24±0.25±0.25±0.29±0.29±0.36±0.36±0.42±0.42
5.0 – 6.0±0.20±0.20±0.24±0.24±0.25±0.25±0.26±0.26±0.32±0.32±0.40±0.40±0.46±0.46
6.0 – 8.0±0.24±0.24±0.30±0.30±0.31±0.31±0.32±0.32±0.38±0.38±0.44±0.44±0.50±0.50
8.0 – 10±0.27±0.27±0.33±0.33±0.36±0.36±0.38±0.38±0.44±0.44±0.50±0.50±0.56±0.56
10 – 12±0.32±0.32±0.38±0.38±0.40±0.40±0.41±0.41±0.47±0.47±0.53±0.53±0.59±0.59
12 – 15±0.36±0.36±0.42±0.42±0.43±0.43±0.45±0.45±0.51±0.51±0.57±0.57±0.63±0.63
15 – 20±0.38±0.38±0.44±0.44±0.46±0.46±0.48±0.48±0.54±0.54±0.60±0.60±0.66±0.66
20 – 25±0.40±0.40±0.46±0.46±0.48±0.48±0.50±0.50±0.56±0.56±0.62±0.62±0.68±0.68
25 – 30±0.45±0.45±0.50±0.50±0.53±0.53±0.55±0.55±0.60±0.60±0.65±0.65±0.70±0.70
30 – 40±0.50±0.50±0.55±0.55±0.58±0.58±0.60±0.60±0.65±0.65±0.70±0.70±0.75±0.75
40 – 50±0.55±0.55±0.60±0.60±0.63±0.63±0.65±0.65±0.70±0.70±0.75±0.75±0.80±0.80

When measuring thickness, a 10 mm zone from the product edges is disregarded (EN 485-4:1993).

Width
Tolerance values are confirmed according to the selected product specification and applicable standard.
Length
Not applicable — coils are supplied continuous / by weight, not cut length.
Straightness
Tolerance values are confirmed according to the selected product specification and applicable standard.
04

Temper Designations & Heat Treatment

Temper DesignationGeneral MeaningTypical Effect on PropertiesCommon Product Forms
FAs fabricated — no special control over strain-hardening or heat treatmentProperties not guaranteed, depend entirely on the forming processAny product form, as it comes off the mill/press
OAnnealed / fully soft conditionLowest strength, highest ductility and formabilitySheet, coil
HStrain-hardened (work-hardened, non-heat-treatable alloys)Strength increases, ductility decreases, with sub-classes (e.g. H14, H24) indicating degree of hardeningSheet, coil, plate
WSolution heat-treated — unstable temperApplies only between solution treatment and natural/artificial ageing; properties change over timeHeat-treatable alloys in transit to a T temper
TThermally treated (heat-treatable alloys), with sub-classes (e.g. T6, T66) indicating the specific heat-treatment/ageing sequenceHigher strength and hardness versus as-fabricated condition; exact levels depend on alloy and processExtruded bar, profiles, plate

Temper availability depends on the alloy, product form, supplier, and order requirements.

05

Standards Cross-Reference

Aluminum AlloyAA DesignationASTM ReferenceEN ReferenceISO ReferenceProduct FormNotes
1050AA1050—EN AW-1050, EN 485/515/573—Sheet/CoilCertified per EN 10204-3.1B
3003AA3003—EN AW-3003, EN 485/515/573—Sheet/CoilCertified per EN 10204-3.1B
5005AAA5005A—EN AW-5005A, EN 485/515/573—PlateEN 10204-3.1 / EN 15088:2005
5083AA5083—EN AW-5083—Coil/SheetComposition per company spec
6082AA6082—EN AW-6082, EN 573-3, EN 755-2—Bar/ExtrusionT6 temper
6061AA6061—EN AW-6061, EN 573-3, EN 755-2—Bar/ExtrusionT6 temper
6063AA6063—EN AW-6063, EN 573-3, EN 755-2—Bar/ExtrusionT66 temper
6060AA6060—EN AW-6060, EN 573-3, EN 755-2—Bar/ExtrusionT66 temper
7075AA7075—EN AW-7075, EN 573-3, EN 755-2, EN 755-5—Extruded flat barT6 temper, certified per EN 10204-3.1

Standards and designations must be confirmed for each product, alloy, temper, and order requirement.

Need this against your specification?

Send us your alloy, temper, form, and dimensions and our technical team will confirm availability, tolerances, and applicable standards.

Request a Quote